Low-Fire Processing of Voltage-Tunable Ba0.6sr0.4tio3 Dielectric

Yu Lu,Jau-Ho Jean
DOI: https://doi.org/10.1143/jjap.46.3481
2007-01-01
Abstract:By adding a low-softening-point Li2O–B2O3–SiO2–CaO–Al2O3 (LBSCA) glass, the voltage-tunable Ba0.6Sr0.4TiO3 (BST64) ceramics can be densified at 900 °C, which is 400–500 °C lower than the temperature for producing the pure BST64. This is caused by liquid-phase sintering and an interfacial reaction taking place at the interface of LBSCA/Ba0.6Sr0.4TiO3. For the samples with 10–35 vol % LBSCA glass, a high relative sintered density of >95% is obtained at 900 °C and the resulting dielectric composites have a dielectric constant and loss at 1 MHz in the ranges of 1040–145 and 0.4–1.0%, respectively. The voltage tunability of the resulting LBSCA+BST64 dielectric at 1 MHz and 1 kV/mm is in the range of 0.8–8%, which exhibits a decreasing trend with increasing LBSCA content.