Preparation and Properties of the C-Shaped SiC Fibers

Liu Xuguang,Wang Yingde,Jiang Yonggang,Wang Deyin,Zhang Xiaobin
DOI: https://doi.org/10.3321/j.issn:1002-185X.2008.z1.102
2008-01-01
Rare Metal Materials and Engineering
Abstract:C-shaped SiC fibers were fabricated by the process of melt-spinning, curing and pyrolysis. Dp of the C-shaped SiC fibers was determined to be 0.3, Ed was 27 mu m, and the tensile strength was 1.5 GPa. In X-wave, epsilon' of C-shaped SiC fibers was between 8.79 and 9.15, epsilon " between 4.70 and 5.94, and tan delta between 0.52 and 0.65. The C-shaped SiC fibers appeared as dielectric loss materials, and exhibited good properties of absorbing electromagnetic waves.
What problem does this paper attempt to address?