Microstructures and Corrosion Properties of Nanocrystalline Cu Coatings Synthesized by Electroless Plating

Zhang Hanzhuo,Fang Liang,Zhou Yaguo,Shi Gaoliang
2012-01-01
Rare Metal Materials and Engineering
Abstract:Nanocrystalline Cu coatings with dense and glossy surfaces were produced on quartz glass substrates by an electroless plating technique. By increasing the electroless time from 10 min to 60 min, the average grain size of nanocrystalline Cu coatings is increased from 22 nm to 75 nm, with a weakened (111) texture and a higher degree of surface roughness. Corrosion properties of both nanocrystalline Cu coatings and coarse-grained Cu were compared and investigated by polarization curves and immersion tests. The results indicate that nanocrystalline Cu coatings have an improved corrosion resistance in 3.5% NaCl solution. Its failure is attributed to the corrosion solution penetrating into the interface between the coatings and the glass substrates through pitting cavities. In 10% NaOH solution, however, nanocrystalline Cu coatings are easier to corrode and prone to form microcracks quickly due to the stress corrosion cracking.
What problem does this paper attempt to address?