Abstract:The corrosion products and G20 pipe were tested by SEM and XRD in order to found the reason of the low temperature heating surfaces of biomass boiler in the high temperature gas leaked out in a short time.It was founded that the pit corrosion which speed increased with the heating surface temperature was caused by chlorine.The heating surface could leak out in a short time because of the pit corrosion even though the operation temperature was below than 400 ℃.The chlorine pit corrosion could been lightened by avoid the biomass ash deposit in the surface.