Investigation of damage on FeCr26Ni36Co15W5 alloy reduction furnace tube during service

Jingfeng Guo,Xiangping Guo,Wenwen Liu,Guobing Hu
DOI: https://doi.org/10.1080/09603409.2024.2411872
2024-10-09
Materials at High Temperatures
Abstract:The microstructure and mechanical properties of tungsten powder reduction furnace tube are investigated in this work. After service, the lamellar and skeleton-shape primary carbides of FeCr26Ni36Co15W5 alloy coarsened and formed a continuous network, much fine secondary carbide precipitated in the dendrite interior. The tensile strength and ductility of FeCr26Ni36Co15W5 alloy decreased. And, the creep strength of FeCr26Ni36Co15W5 alloy has reached the end of the service life. Meanwhile, the corrosion products were studied by XRD and XRF. It was found that the corrosion products were Na 2 WO 4 ·2 h 2 O, Na 2 CO 3 ·H 2 O and Cr 4 Ni 15 W,and the evaporation of catalyst (Na 2 CO 3 ) results in a large amount of Na 2 CO 3 ·H 2 O in the corrosion products. The hot corrosion mechanism of the reduction furnace tube is Type I hot corrosion.
materials science, multidisciplinary,metallurgy & metallurgical engineering
What problem does this paper attempt to address?