Elemental distribution and fracture properties of magnetron sputtered carbon supersaturated tungsten films

S. Fritze,R. Hahn,H. Aboulfadl,F.O.L. Johansson,R. Lindblad,K. Böőr,A. Lindblad,E. Berggren,D. Kühn,T. Leitner,B. Osinger,E. Lewin,U. Jansson,P.H. Mayrhofer,M. Thuvander
DOI: https://doi.org/10.1016/j.surfcoat.2023.130326
IF: 4.865
2024-01-01
Surface and Coatings Technology
Abstract:The combination of strength and toughness is a major driving force for alloy design of protective coatings, and nanocrystalline tungsten (W)-alloys have shown to be promising candidates for combining strength and toughness. Here we investigate the elemental distribution and the fracture toughness of carbon (C) alloyed W thin films prepared by non-reactive magnetron sputtering. W:C films with up to ~4 at.% C crystallize in a body-centered-cubic structure with a strong 〈hh0〉texture, and no additional carbide phases are observed in the diffraction pattern. Atom probe tomography and X-ray photoelectron spectroscopy confirmed the formation of such a supersaturated solid solution. The pure W film has a hardness ~13 GPa and the W:C films exhibit a peak hardness of ~24 GPa. In-situ micromechanical cantilever bending tests show that the fracture toughness decreases from ~4.5 MPa·m 1/2 for the W film to ~3.1 MPa·m 1/2 for W:C films. The results show that C can significantly enhance the hardness of W thin films while retaining a high fracture toughness.
physics, applied,materials science, coatings & films
What problem does this paper attempt to address?