Impact of Interlayer and Ferroelectric Materials on Charge Trapping During Endurance Fatigue of FeFET With TiN/Hf x Zr 1- x O 2 /Interlayer/Si (MFIS) Gate Structure
Fengbin Tian,Shujing Zhao,Hao Xu,Jinjuan Xiang,Tingting Li,Wenjuan Xiong,Jiahui Duan,Junshuai Chai,Kai Han,Xiaolei Wang,Wenwu Wang,Tianchun Ye
DOI: https://doi.org/10.1109/ted.2021.3114663
IF: 3.1
2021-11-01
IEEE Transactions on Electron Devices
Abstract:We study the impact of different interlayers (ILs) and ferroelectric materials on charge trapping during the endurance fatigue of Si ferroelectric field effect transistor (FeFET) with TiN/HfxZr1-xO2/ interlayer/Si (MFIS) gate-stack. We have fabricated FeFET devices with different interlayers (SiO2 or SiON) and HfxZr1-xO2 materials (${x} =0.75$ , 0.6, 0.5) and directly extracted the charge trapping during endurance fatigue. We find that: 1) under the same equivalent oxide thickness (EOT) condition, the increase of dielectric constant and interlayer thickness suppresses charge trapping and improves the endurance characteristics; 2) charge trapping effect is experimentally verified to be the origin of endurance fatigue; and 3) as the spontaneous polarization (${P}_{\text {s}}{)}$ of the HfxZr1-xO2 decreases from $25.9~ \boldsymbol {\mu } \text{C}$ /cm2 (Hf0.5Zr0.5O2) to $20.3~ \boldsymbol {\mu } \text{C}$ /cm2 (Hf0.6Zr0.4O2), the charge trapping behavior decreases, resulting in the slow degradation rate of memory window (MW) during program/erase cycling; in addition, when ${P}_{\text {s}}$ further decreases to $8.1~ \boldsymbol {\mu }\text{C}$ /cm2 (Hf0.75Zr0.25O2), the initial MW nearly disappears (only ~0.02 V). Thus, the reduction of ${P}_{\text {s}}$ could improve endurance characteristics. On the contrary, it can also reduce the MW. Our work helps design the MFIS gate-stack to improve endurance characteristics.
engineering, electrical & electronic,physics, applied