Enhancing Textile Cotton Yarn Sizing: Investigating Factors Impacting Breaking Strength, Pick-Up Percentage, and Elongation Loss
Derseh Yilie Limeneh,Million Ayele,Mesfin Shiferaw Wubie,Addisu Ferede Tessema,Noureddine Abidi,Zelalem Adane Alemar
DOI: https://doi.org/10.1080/15440478.2024.2356691
2024-05-28
Journal of Natural Fibers
Abstract:The paper investigates the effect of machine setting on breaking strength, breaking elongation, and pick-up percentage of sized yarn properties. The factors considered are concentration of size solution, squeezing pressure and counts of yarn, the aim to develop a regression model that shows the effect of factors on size pick-up percentage, breaking strength regain, and loss in breaking elongation. The experiment is conducted by using 16 Ne and 21 Ne of cotton yarn, 3 Bar and 5 Bar of squeezing pressure, and 1.9% and 6% of size concentration with maize starch as sizing agent. A factorial design with two factors and 5 replicants has been used to design the experiment and analyze the results. The result showed that a slight change in squeezing pressure and concentration significantly affects the pick-up percentage, breaking strength regain and breaking elongation loss while a change of yarn count would not have a significant effect on the pick-up percentage of sized yarn. Furthermore, for achieving optimum properties of the sized yarn the pressure of squeezing, the count of the yarn and the concentration of the solution should be adjusted, and a regression model is developed to investigate the properties of the sized yarn by considering considered factors. 研究了棉纱上浆过程中机器设置对浆纱断裂强力、断裂伸长率和上浆纱性能的影响. 本研究考虑的因素是浆料浓度、挤压压力和纱线支数. 本研究旨在建立一个回归模型,显示使用不同支数的纱线、挤压压力、浆料浓度对浆料的上浆率、断裂强力回复率和断裂伸长率损失的影响. 实验在Else Addis Industrial PLC中进行,使用16 Ne和21 Ne的纱线支数,3巴和5巴的挤压压力,以及1.9%和6%的浆料浓度,使用玉米淀粉作为施胶剂. 采用两因素和5个重复因子的因子设计对实验进行设计并对结果进行分析. 分析结果表明,挤压压力和浆料浓度的微小变化对上浆纱的拾取率、断裂强力回复率和断裂伸长率损失有显著影响,而纱线支数的变化对上浆纱线的拾取率没有显著影响. 此外,为了获得上浆纱的最佳性能,应调整挤压压力、纱线数量和溶液浓度,并通过考虑因素建立回归模型来研究上浆纱的性能.
materials science, textiles