Effect of heat treatments on microstructure and mechanical properties of sand cast Al–2Li–2Cu–0.5Mg–0.2Sc–0.2Zr alloy

Jin-shuo ZHANG,Xiao-xiang ZHONG,Liang ZHANG,Guo-hua WU,Wen-cai LIU
DOI: https://doi.org/10.1016/s1003-6326(22)65803-5
IF: 3.752
2022-02-01
Transactions of Nonferrous Metals Society of China
Abstract:This study focused on modifying heat treatment schemes to enhance the mechanical properties of sand cast Al–2Li–2Cu–0.5Mg–0.2Sc–0.2Zr alloy. Different three-stage solution treatment schemes ((460 °C, 32 h) + (520 °C, 24 h) + (530/540/550 °C, 4/12/24/32 h)) and aging temperatures (125, 175, 225 °C) were designed for comparison. The microstructure evolutions were analyzed by optical microscopy (OM), scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The results showed that the three-stage solution treatment of (460 °C, 32 h) + (520 °C, 24 h) + (530 °C, 12 h) could dissolve most of the secondary phases. The TEM results illustrated that fine δ’(Al3Li) particles were homogeneously distributed in the matrix after aging at 175 °C for 8 h, accompanied by a small amount of lath-shaped S′(Al2CuMg) and plate-like T 1(Al2CuLi) phases. The best comprehensive properties of yield strength of 376 MPa, ultimate tensile strength of 458 MPa and elongation of 4.1% were obtained by the optimal heat treatment scheme ((460 °C, 32 h) + (520 °C, 24 h) + (530 °C, 12 h) + (175 °C, 8 h)).
metallurgy & metallurgical engineering
What problem does this paper attempt to address?