HfO2 doped 3Y-TZP on mechanical properties and low temperature degradation (LTD)

Liu Zhang,Haiqing Yin,Binbin Rong,Ruijie Zhang,Cong Zhang,Xue Jiang,Yongwei Wang,Xuanhui Qu
DOI: https://doi.org/10.1016/j.ceramint.2024.02.277
IF: 5.532
2024-02-01
Ceramics International
Abstract:The mechanical properties and ageing resistance of 0.5–10 mol% HfO2 doped 3Y-TZP have been investigated. All samples were sintered at 1500 ◦C-2 h and characterized by density testing. Samples with polished surfaces were submitted to X-Ray diffraction (XRD) and microstructure testing and then cut into standards for 3-point bending testing. Group 2 was characterized by Vickers hardness and fracture toughness. Group 3 was accelerated ageing procession in autoclave condition containing at 134 °C and 0.2 MPa 10 h up to 40 h, and then detected by transmission electron microscopy (TEM) analysis. All sintered specimens presented nearly full densification. The grain size of 3Y0.5Hf-TZP was smaller than that of undoped 3Y-TZP after sintering. 3Y0.5Hf-TZP enhanced the bending strength by 34.6% compared to 3Y-TZP. The ageing kinetic parameter (n ∼ (0.66–1.64)) was related to the grain size and the ageing time from the onset of the transition until the transition reaches saturation.
materials science, ceramics
What problem does this paper attempt to address?