Structure and properties of La 0.6 Ce 0.3 Pr 0.1 B 6 ‐ZrB 2, a directionally solidified eutectic with different growth rates
Feng Shi,Danmin Liu,Yan Wang,Linlin Liu,Weiqiang Xiao,Cuixiu Liu,Xinyu Yang,Jiuxing Zhang
DOI: https://doi.org/10.1111/jace.18040
IF: 4.186
2021-08-09
Journal of the American Ceramic Society
Abstract:<p>La<sub>0.6</sub>Ce<sub>0.3</sub>Pr<sub>0.1</sub>B<sub>6</sub>-ZrB<sub>2,</sub> a directionally solidified eutectic (DSE), is a material with a high-performance thermionic emission with great application prospects. The influence of the growth rates of this DSE on the microstructure, growth direction, two phases orientation relationship, mechanical properties, and thermionic emission properties were investigated. The experimental results show that the microstructure and growth direction of the two phases varied with the growth rate of the eutectic: the faster the growth rate, the lower the uniformity of the ZrB<sub>2</sub> phase became, and the growth directions of the La<sub>0.6</sub>Ce<sub>0.3</sub>Pr<sub>0.1</sub>B<sub>6</sub> matrix and the ZrB<sub>2</sub> phase were also altered accordingly. In the La<sub>0.6</sub>Ce<sub>0.3</sub>Pr<sub>0.1</sub>B<sub>6</sub>-ZrB<sub>2</sub> DSE with a growth rate of 100 mm/h the two phases have a unique growth direction and a crystallographic orientation relationship. The fracture toughness of the La<sub>0.6</sub>Ce<sub>0.3</sub>Pr<sub>0.1</sub>B<sub>6</sub>-ZrB<sub>2</sub> DSE is at least 50% higher than that of the single crystal La<sub>0.6</sub>Ce<sub>0.3</sub>Pr<sub>0.1</sub>B<sub>6</sub>, and the fracture toughness of the DSEs formed at different growth rates also differed.</p>
materials science, ceramics