Effects of the Simultaneous Addition of Gd and Mn on the Microstructures and Mechanical Properties of Mg-Bi Alloys

Bingchun Jiang,Jun Zhao,Yang Liu,Yanfu Chai,Liwei Lu
DOI: https://doi.org/10.1007/s11665-023-09112-9
IF: 2.3
2024-01-10
Journal of Materials Engineering and Performance
Abstract:This study investigated the effect of the synergistic addition of Gd and Mn on the microstructure and mechanical properties of extruded Mg-1Bi alloys. The grain size of an Mg-1Bi alloy decreased sharply when either only Gd or Mn was added to the alloy, whereas a strong grain refining effect was verified upon the co-addition of Gd and Mn. The Mg-1Bi and Mg-1Bi-0.4Mn alloys exhibited typical strong basal textures, whereas the Mg-1Bi-0.3Gd and Mg-1Bi-0.3Gd-0.6Mn alloys showed weakened extrusion direction (ED)-split textures. The weakened ED-split texture leads to a high average Schmid factor for basal slip (SF b ). Higher SF b for the sheet exhibited the lower yield strength and higher ductility. Furthermore, the synergistic addition of Gd and Mn resulted in considerably higher strength and ductility than the addition of either Gd or Mn alone. The Mg-1Bi-0.3Gd-0.6Mn sheet shows the ultimate tensile and yield strengths of ~ 275.6 and ~ 180.2 MPa along the transverse direction (TD) and ~ 273.2 and ~ 155.4 MPa along the extrusion direction (ED), respectively. Moreover, the elongation of Mg-1Bi-0.3Gd-0.6Mn sheet along the TD and ED increased to ~ 7.3 and ~ 7.5%, respectively, more than two times compared with the corresponding values for the Mg-1Bi sheet. The increased yield strength of the Mg-1Bi-0.3Gd-0.6Mn sheet was mainly attributed to the effect of refined grain size, fine α-Mn and MgBiGd particles, and the Gd solute. In addition, the ductility of the Mg-1Bi-0.3Gd-0.6Mn sheet was substantially increased because of the fine grain size and weak texture having a high average SF b .
materials science, multidisciplinary
What problem does this paper attempt to address?