Improvement of adhesion under the scratching condition for diamond film on the steel by adding a precarbonization process

Xiao Li,Hao Chen,Chengcheng Wang,Chengke Chen,Meiyan Jiang,Xiaojun Hu
DOI: https://doi.org/10.1016/j.diamond.2023.109927
IF: 3.806
2023-04-21
Diamond and Related Materials
Abstract:Diamond films deposited on the stainless steel using a Cr/Cr-Si-N interlayer exhibited good adhesion in the Rockwell C indentation, while these films showed a very low critical load under the scratch test, which limits its application in medical devices with a relative motion. In order to solve this problem, we introduce a precarbonization process for the Cr/Cr-Si-N interlayer before the deposition of diamond films, which obviously improves the adhesion under the scratch test of diamond films. Especially, when the precarbonization time is 5 min, the critical load for diamond film under the scratch test reaches 26.6 ± 1.0 N, which is ascribed to the addition of precarbonization process changing the growth of the carbide , resulting in the elimination of pores under the diamond/carbide interface and the formation of jagged interface structure induced mechanical interlocking effect.
materials science, multidisciplinary,physics, applied, condensed matter, coatings & films
What problem does this paper attempt to address?