Dry Cold Forging of High Strength AISI316 Wires by Massively Nitrogen Supersaturated CoCrMo Dies

Tatsuhiko Aizawa,Tatsuya Fukuda,Tomomi Shiratori
DOI: https://doi.org/10.3390/pr12112561
IF: 3.5
2024-11-23
Processes
Abstract:The plasma immersion nitriding system was utilized to make massive nitrogen supersaturation (MNS) to CoCrMo disc and die substrates at 723 K for 21.6 ks. The top layer thickness in the multi-layered MNSed layer was 20 μm. Its nitrogen solute content reached 5 mass% on average after SEM-EDX analysis. The surface hardness was 1300 HV1N (HV0.1), which was much higher than the bare CoCrMo with 450 HV1N. The original polycrystalline structure was modified to be a multi-layered microstructure, which consisted of the nanograined MNSed top layer, the buffer layer with a thickness of 5 μm, and the column–granular structured layer with their textured crystallographic orientations. The BOD (ball-on-disc) testing was employed to describe the frictional sliding behavior under the applied loads of 5 N and 10 N and the sliding velocity of 0.1 m/s against the AISI316 ball. The friction coefficient was held constant by 0.68 on average. The CNC (Computer Numerical Control) stamping system was employed to upset the fine-grained 1.0 mm thick AISI316 wire up to 70% in reduction in thickness. The friction coefficient at RT was estimated to be 0.05. A round, fine-grained AISI316 wire was shaped into a thin plate with a thickness of 0.3 mm in cold and dry.
engineering, chemical
What problem does this paper attempt to address?