Hot corrosion resistance of oxide‐doped yttria‐stabilized zirconia powder in V2O5 molten salt

Nestor K. Ankah,Zuhair M. Gasem
DOI: https://doi.org/10.1002/maco.202414291
2024-03-27
Materials and Corrosion
Abstract:This study explores the use of alkaline‐earth oxides and transition metal oxides to improve the hot corrosion resistance of 8 wt.% yttria‐stabilized zirconia (8YSZ). The effects of doping on pure and blended 8YSZ materials are investigated at elevated temperatures. Results show improved performance, with outcomes dependent on temperature and dopant concentration. The study provides valuable insights into the development of 8YSZ‐based materials with enhanced performance against hot corrosion. The hot corrosion resistance of 8 wt.% yttria‐stabilized zirconia (8YSZ) powder, modified with CaO, MgO, Ta2O5, and TiO2 at concentrations of 5, 10, and 15 wt.%, was systematically investigated in a molten vanadium pentoxide (V2O5) environment at 900°C and 1100°C for 48 h. The modified 8YSZ samples, coated with V2O5, underwent thermal cycling totaling 12 cycles. Results revealed susceptibility to hot corrosion for all doped 8YSZ powders, attributed to tetragonal ZrO2 destabilization, forming monoclinic ZrO2. Remarkably, 8YSZ/CaO demonstrated exceptional resistance to hot corrosion when exposed to a temperature of 900°C. The corrosion product found in the 8YSZ/Ta2O5 material was determined to be tetragonal Zr0.66Y0.17Ta0.17O2. Although, 8YSZ/TiO2 undergoes deterioration at 900°C, it exhibits improved resistance at 1100°C, resulting in the formation of TiVO4.
materials science, multidisciplinary,metallurgy & metallurgical engineering
What problem does this paper attempt to address?