The simultaneous improvement of strength and ductility of the 93W-4.6Ni-2.4Fe prepared by additive manufacturing via optimizing sintering post-treatment

Zhangping Hu,Ye Liu,Jin Wu,Ji Dong,Zongqing Ma,Yongchang Liu
DOI: https://doi.org/10.1016/j.addma.2021.102216
IF: 11
2021-10-01
Additive Manufacturing
Abstract:The influence of sintering post-treatment temperature on the microstructure and mechanical properties of 93 W-4.6Ni-2.4Fe (wt%) tungsten heavy alloy prepared by powder extrusion 3D printing has been examined. The density of the specimen gradually increases to over 99.5% with the increase of the sintering temperature. The contiguity first decreases with increasing temperature and then increases, which is mainly related to the evolution of the distribution of γ phase and the tungsten particle size. The fracture mode of the 93W-4.6Ni-2.4Fe specimen changes from brittle fracture for the sintering temperature of 1430 °C to ductile fracture for the sintering temperature range of 1450–1480 °C. The sintering temperature of the 93 W-4.6Ni-2.4Fe specimen with the highest tensile strength (1040 ± 6 MPa) and elongation (20.7 ± 0.4%) is determined to be 1480 °C. The high ductility of the specimen sintered at 1480 °C can be attributed to the formation of high-density uniformly distributed dimples in the network γ phase and the bridging effect of γ phase on the cracks. The high strength is related to the high density of specimen, moderate contiguity, suitable tungsten particle size and solid solution strengthening effect.
engineering, manufacturing,materials science, multidisciplinary
What problem does this paper attempt to address?