Abstract:Elemental powder (EP) sintering is attractive for use in fabricating the NiTi shape memory alloys due to its low cost and compositional flexibility. However, because of sintering challenges that are not adequately resolved, current EP NiTi alloys exhibit zero or trace tensile properties. In this study, a 10−4 Pa vacuum system was used to optimize the sintering of EP NiTi alloys. The unavoidable liquid phase and high-temperature sintering promoted elemental homogenization, which substantially improved the engineering properties of EP NiTi. Compared to previous studies, increasing the vacuum level caused deflagration reactions at a low temperature of 700 °C. It also rendered the materials more susceptible to macroscopic millimeter-scale defects at > 1050 °C due to the loss of the liquid phase. These problems could be avoided by optimizing the sintering process and completing high-temperature sintering at 1250 °C. High-temperature sintering promoted local elemental homogenization rather than extensive elemental migration. 3D–Computed Tomography reconstruction revealed that high-temperature sintering promoted shrinkage of the pore volumes and homogeneity of pore size distribution. This sintering process considerably improved the mechanical properties of the EP NiTi alloy. The tensile strength and related elongation were 701–763 MPa and 16.54–21.97%, respectively, and the alloy exhibited a shape memory of >90% in an 8% tensile evaluation. This optimization strategy, which integrates impurity control and the intermetallic phase sequence, promotes the practical applications of EP NiTi alloys.
materials science, multidisciplinary,nanoscience & nanotechnology,metallurgy & metallurgical engineering
What problem does this paper attempt to address?