The effects of powder size and sintering temperature on the microstructure and properties of modified MA6000 alloy produced by spark plasma sintering

Dinh Van Cong,Dong-Wan Lee,Su-Gwan Lee,Jin-Woo Kim,Hwi-Jun Kim,Joong-Gyeong Lim,Tae-Shik Yoon,Jin-Chun Kim
DOI: https://doi.org/10.1080/00325899.2023.2230693
IF: 2.2281
2023-07-04
Powder Metallurgy
Abstract:The present study investigates the properties and microstructure evolution of MA 6000, a nickel-based alloy produced by mechanical alloying and spark plasma sintering (SPS), a powder processing technique in metallurgy. This study aims to explore the potential of MA 6000 as a high-temperature material for industrial applications. Modified MA 6000 samples of different powder sizes were sintered in a high-vacuum environment at temperatures ranging from 800 to 1100°C. At 800°C, the cohesion between powder particles was not significant, resulting in low-density samples. However, at 1000°C, the samples consisted of many fully sintered regions related to finer powder particles, while no specific morphology was observed at 1050°C. The image quality and inverse pole figure (IQ-IPF) map indicated that the grains were distributed randomly in all sintered samples, and the average distribution of grain size of samples sintered at 1050°C was larger than that of those sintered at 1000°C.
metallurgy & metallurgical engineering
What problem does this paper attempt to address?