Flexural strength of novel glass infiltrated monochrome and multilayer high yttrium oxide containing zirconia upon various sintered cooling rates

Pithiwat Uasuwan,Niwut Juntavee,Apa Juntavee
DOI: https://doi.org/10.1111/jopr.13872
2024-06-04
Journal of Prosthodontics
Abstract:Purpose The sintering technique and cooling strategy influence the strength of zirconia. This study examined the impact of altering the cooling rate of glass‐infiltrated monolayer and multilayer 5 mol% yttria‐partially stabilized zirconia (5Y‐PSZ) on their strength. Materials and Methods One‐hundred eighty (180) specimens (width × length × thickness = 10 × 20 × 2 mm) were prepared using monolayer (Mo: Cercon‐xt) and multilayer (Mu: Cercon‐xt ML) 5Y‐PSZ. Randomly distributed specimens (n = 15/group) were sintered with traditional (T) versus glass infiltrated (G) technique and cooled down with different cooling rates: slow (S: 5°C/min), normal (N: 35°C/min), and fast (F: 70°C/min). Four‐point bending test was used to measure flexural strength (σ). Microstructures were investigated by scanning electron microscope (SEM), energy dispersive spectroscopy (EDS), and X‐ray diffraction (XRD). Three‐way ANOVA and Tamhane comparisons were determined for a significant difference of σ (p
dentistry, oral surgery & medicine
What problem does this paper attempt to address?