Effect of heat treatment on microstructure and mechanical properties of Cu–6.9Ni–2.97Al–0.99Fe–1.06Mn alloy

Ran Yang,Jiuba Wen,Yanjun Zhou,Kexing Song,Liye Niu,Huiwen Guo,Yan Yu
DOI: https://doi.org/10.1080/02670836.2019.1684035
IF: 1.8
2019-11-03
Materials Science and Technology
Abstract:The effect of heat treatment on the mechanical properties and microstructures of Cu–6.9Ni–2.97Al–0.99Fe–1.06Mn alloys was investigated. The results show that the microstructure of the as-cast alloy mainly consists of an alpha-copper matrix and γ-phase Ni<sub>3</sub>Al particles. The microstructure of the alloy after solution treatment at 950°C for 2 h is a single-phase alpha-copper supersaturated solid solution and the second-phase strengthening disappears. After ageing treatment at 550°C for 6 h, the γ-phase particles are fully precipitated, and the mechanical properties of the alloy are significantly improved. The tensile strength is increased from 305 to 588 MPa. Quasi-cleavage fracture with shallow dimples appeared in the Cu–6.9Ni–2.97Al–0.99Fe–1.06Mn alloy aged at 550°C for 6 h.
materials science, multidisciplinary,metallurgy & metallurgical engineering
What problem does this paper attempt to address?