Improvement of Mechanical Strength of 8 mol % Yttria-Stabilized Zirconia Ceramics by Spark-Plasma Sintering

Tomonari Takeuchi,Isao Kondoh,Nobuyuki Tamari,Nalini Balakrishnan,Katsuhiro Nomura,Hiroyuki Kageyama,Yasuo Takeda
DOI: https://doi.org/10.1149/1.1456915
IF: 3.9
2002-01-01
Journal of The Electrochemical Society
Abstract:Dense 8 mol % yttria-stabilized zirconia (8YSZ) ceramics consisting of submicrometer-sized grains were prepared using the spark-plasma sintering (SPS) method without any additives. The starting powder (ca. 0.1 μm) was densified to ca. 99% of the theoretical X-ray density with shorter sintering time (5-10 min) while preserving a grain size in submicrometer. The measured three-point bending strength was ca. 400 MPa at room temperature for samples sintered at 1300°C for 5-10 min, which was higher than the value of conventionally sintered ceramics, ca. 250 MPa, due mainly to the small-grained microstructures of the SPS ceramics. The electrical conductivity was 0.19 S cm−1 at 1000°C in air, which is comparable to previously reported values (ca. 0.1 S cm−1) for well-sintered ceramics. Thus, the SPS method is an effective process to improve the mechanical strength of 8YSZ without degrading the electrical conductivity. © 2002 The Electrochemical Society. All rights reserved.
electrochemistry,materials science, coatings & films
What problem does this paper attempt to address?