Slag formation path in converter smelting process of semi-steel containing chromium

Jiang Diao,Wenfeng Gu,Liang Liu,Wenfeng Tan,Hongyi Li,Bing Xie
DOI: https://doi.org/10.1080/03019233.2020.1737791
2020-03-13
Abstract:Aiming at the high-efficiency utilization of vanadium–titanium magnetite with high chromium content, a slag formation path in the converter smelting process of semi-steel containing chromium was proposed. The influences of MnO and Cr2O3 on the melting characteristics of converter slag were calculated through FactSage. The effects of components and temperature on the equilibrium distribution ratio of P, Cr between molten CaO–SiO2–FeO–MgO–MnO–Cr2O3–P2O5 slags and molten steel was obtained by the indirect experimental method and the regular solution model. The results show that the liquidus region and the proportion of liquid phase decrease with the increase of Cr2O3 content in steel slag. The increases of basicity conduces to dechromization and dephosphorization. The LCr increased continuously with increasing FeO content and the influence of the oxidization of steel slag on the LCr is greater than LP. Both LP and LCr decrease distinctly with the increase in temperature. The slag formation path for the smelting process of semi-steel containing chromium is as follows: 17wt-%CaO–16wt-%SiO2–67wt-%FeO→25wt-%CaO–20wt-%SiO2–55wt-%FeO→57wt-%CaO–17wt-%SiO2– 6wt-%FeO.
metallurgy & metallurgical engineering
What problem does this paper attempt to address?