Abstract:High temperature stability (1100-1500 °C) and oxidation behavior at 1500 °C of the SiOC/HfO2 ceramic nanocomposite were investigated in air. Consumption of free carbon in bulk dominated the thermal stabilities at below 1200 °C. Whereas, the continuous cristobalite scale, rather than HfSiO4, was responsible for the improved oxidation resistance at exceeding 1200 °C. At 1500 °C, HfSiO4, with maximum 30 vol. % content for critical duration of ∼ 15 h, suffered ruptured spherical-bubbles by volatilized species and did not consolidate into a complete protective scale. Thus, the bulk exhibited limited resistance to oxidation at 1500 °C for long-term applications.