Hot-injection for synthesizing ammonium thiosulfate precursor of molybdenum disulfide thin film coated on nano-porous aluminum oxide for surface strengthening

Lung-Hao Hu,Po-Chun Chen
DOI: https://doi.org/10.1016/j.jallcom.2020.156262
IF: 6.2
2020-12-01
Journal of Alloys and Compounds
Abstract:<p>A cheap and massive producible ammonium thiosulfate precursor has been synthesized by hot-injection method for coating MoS<sub>2</sub> layer onto the nano-porous anodic aluminum oxide (AAO) layer on the surface of 7003 alloy. The ammonium thiosulfate precursor is pyrolyzed at 280, 375, 400 and 550 °C to form the MoS<sub>2</sub> layer, respectively. After 1440 m wear test, the wear rates (weight loss/Original weight) of pure 7003 alloy, anodized 7003 alloy and MoS<sub>2</sub> coated 7003 alloy pyrolyzed at 400 °C are 0.339%, 0.017%, and 0.0109%, respectively. The thickness of the molybdenum disulfide film observed by transmission electron microscope is about 43.3 nm. The surface hardness of MoS<sub>2</sub> coated 7003 alloy is about 5–6 Gpa higher than that of AAO, 3–4 Gpa measured by nanoindentation. The maximum reduced modulus of elasticity is about 90 Gpa as the pyrolytic temperature reaches 400 °C. The ratio of the average surface hardness (<em>H*</em>) and reduced modulus of elasticity (<em>E*</em>) is linearly proportional to the elastic recovery rates (<em>W</em><sub><em>e</em></sub>), calculated from the maximum indentation depths with different pyrolytic temperatures. The elastic recovery rate would remain in a range of the pyrolytic temperatures between the occurrence of solid solutionization and completion of the solid solution homogenization for Al–Mo alloy formation.</p>
materials science, multidisciplinary,chemistry, physical,metallurgy & metallurgical engineering
What problem does this paper attempt to address?