Abstract:The Inconel 718 superalloy was fabricated using spark plasma sintering (SPS) technology with varying sintering temperatures and heating rates. The densification and mechanical property of the sintered superalloys were characterized through tensile and compression tests at room temperature, as well as microscopic analyses. The evidence suggests that the plasma generated between the particles results in evaporative melting on the particle surface and plastic deformation of the particle boundaries, accelerating the densification process is by 3 similar to 4 times. Besides, the grain size refinement coefficient affected by pulse current in the holding stage is 0.7-0.8, leading to a significant grain boundary strengthening during SPS process. The dislocation dominated by ball milling and SPS parameters also helps improve the strength and plasticity of the sintered superalloy. The superalloy sintered at 1050 degrees C with a heating rate of 100 degrees C/min demonstrated the highest tensile and compressive fracture strengths, measuring 1410 MPa and 1983 MPa, respectively, with the tensile and compressive yield strength of 712 MPa and 1557 MPa, respectively. Lower sintering temperatures or higher heating rates results in lower levels of densification and decreased strength. In addition, plasticity is reduced at higher sintering temperatures or lower heating rates due to excessive precipitation of brittle phases.
What problem does this paper attempt to address?