Abstract:Here we report for the first time that Magnéli phase Ti 4 O 7 electrode with super performance is successfully prepared by hot-pressed sintering of single-phase submicron Ti 4 O 7 powders. The microstructure, mechanical properties, electrical conductivity and electrochemical performance of the Ti 4 O 7 electrodes were also investigated. Results show that the compact and homogeneous bulk Ti 4 O 7 without evident defects such as pores and cracks is achieved when the submicron Ti 4 O 7 powder was sintered at 1200 °C for 0.5 h. As a result, the bulk density of the Ti 4 O 7 reaches its theoretical value (4.323 g cm −3 ). Additionally, it has excellent physical and chemical properties, including the mean values of hardness and Young's modulus of 15.20 ± 0.42 and 247.40 ± 6.70 GPa, respectively, the Vickers-hardness of 1165.5 ± 9.5 HV, the highest known conductivity of 1252.5 S cm −1 , and the widest known electrochemical stability window of 4.19 V in 1 M NaCl solution.
materials science, ceramics
What problem does this paper attempt to address?