Si-induced Precipitation Modification and Related Age-Hardening Response of an Al–4Mg–1Cu–0.5Si Alloy

Chong Li,Gang Sha,Jun Xia,Yongchang Liu,Simon P. Ringer
DOI: https://doi.org/10.1016/j.matchemphys.2017.01.041
IF: 4.778
2017-01-01
Materials Chemistry and Physics
Abstract:The solid solubility of Si in a quaternary Al–4Mg–1Cu–0.5Si (wt%) alloy has been found to be only about 0.061 at% at 520 °C, and 0.093 at% at 560 °C, less than 1/10 of that in the ternary Al–Mg–Si system. The excess Si in the alloy remains as coarse Mg2Si dispersoids which produce no significant age-hardening effect. Interestingly, a small change of Si content (from 0.061 at.% to 0.093 at.%) in the solid solution of the alloy has been found to be effective in modifying precipitation microstructure by promoting the formation of fine Guinier–Preston–Bagaryasky (GPB) zones and postponing the formation of the S phase during ageing at 200 °C. Consequently, the quaternary alloy exhibits an enhanced age-hardening response during earlier-stage ageing.
What problem does this paper attempt to address?