Densification, Microstructures, and Mechanical Properties of (zr, Ti)(C, N) Ceramics Fabricated by Spark Plasma Sintering

Lanqing Liang,Boxin Wei,Dong Wang,Wenbin Fang,Lei Chen,Yujin Wang
DOI: https://doi.org/10.1016/j.jeurceramsoc.2022.07.012
IF: 5.7
2022-01-01
Journal of the European Ceramic Society
Abstract:Dense (Zr, Ti) (C, N) ceramics were fabricated by spark plasma sintering (SPS) at 1900-2000 degrees C using ZrC, TiCN and ZrH2 powders as raw materials. A single Zr-rich (Zr, Ti)(C, N) solid solution was formed in Zr0.95Ti0.05C0.975N0.025 and Zr0.80Ti0.20C0.90N0.10 ceramics (nominal composition). A Ti-rich solid solution appears in Zr0.50Ti0.50C0.75N0.25 ceramics. The coaddition of TiCN and ZrH2 promoted the densification of (Zr, Ti) (C, N) ceramics by forming solid solutions and carbon vacancies, which could reduce critical resolved shear stress (CRSS) and promote carbon and metal atom diffusion. ZrC-45 mol% TiCN-10 mol% ZrH2 (raw powder composition) possesses good comprehensive mechanical properties (Vickers hardness of 24.5 +/- 0.9 GPa, flexural strength of 503 +/- 51 MPa, and fracture toughness of 4.3 +/- 0.2 MPamiddotm(1/2)), which reach or exceed most ZrC-based (Zr, Ti) C and (Zr, Ti) (C, N) ceramics in previous reports.
What problem does this paper attempt to address?