TERTIARY RECRYSTALLIZATION IN THIN STRIPS OF GRAIN ORIENTED SILICON STEEL PRODUCED BY CROSS SHEAR ROLLING

Gang Liu,Liu Guilan,QI Kemin,Fu Wang,Zuo Liang,Metallurpy,) Shenyang
1998-01-01
Abstract:Commercial grain oriented silicon steel sheet with a thickness of 0.30mm was cold rolled to 0.10mm by the cross shear rolling (CSR) mill with a mismatch speed ratio 1.2 and by the conventional rolling, respectively The thin strips were annealed at 1050℃, 1100℃ and 1150℃ for 5 h in a normal hydrogen atmosphere furnace. It has shown that tertiary recrystallization may occur in the strip produced by the CSR followed by 1050℃ 5h hydrogen annealing, while the grain orientations turn to be parallel to the {110}[001], and the grain size are 1~3mm. As compared the original sheet,the core loss of strip produced by the CSR followed by 1050℃ 5h hydrogen annealing decreases by an amount of 51%, and the magnetic properties are improved significantly. the magnetic properties of this sheet are as follows: B8 = 1.978T, P13/50 = 0.30mW.g-1, P17/50 = 0.72mW.g-1.
What problem does this paper attempt to address?