Recovery of Nickel and Cobalt from Ni-Co-Bearing Purification Slag by Acid-Washing and Reduction Leaching

Wen-ming LIU,Xin-cun TANG,Yang WANG,Yuan JIN,Tao WANG,Le ZHOU,Yi-na WU
DOI: https://doi.org/10.3969/j.issn.1007-7545.2017.05.001
2017-01-01
Abstract:Nickel and cobalt were recovered from Ni-Co-bearing purification residues by acid-washing and reduction leaching.The effects of end point pH value during acid leaching and sulfuric acid content,leaching temperature and time,end point pH value,L/S,and hydrogen peroxide concentration during reduction leaching on leaching rate of Ni and Co were discussed.The results show that nickel leaching rate is 78.1% and cobalt leaching rate is very low under the condition of pH value of 2.5 during acid-washing.Nickel leaching rate is 98.3% and cobalt leaching rate is 97.5% during reduction leaching under the optimum conditions including L/S of 10 ∶ 1,sulfuric acid concentration of 1.5 mol/L,leaching time of 3 h,leaching temperature of 60 ℃,and dosage of hydrogen peroxide of 1.0 mL/g.
What problem does this paper attempt to address?