Hydrogen Storage Characteristics of TiMn1.25-5yCr0.25(V4Fe)y Alloys

余学斌,吴铸,黄太仲
DOI: https://doi.org/10.3321/j.issn:1004-0609.2003.05.013
2003-01-01
Abstract:The reversible hydrogen absorption and desorption behavior of TiMn_(1.25-5y)Cr_(0.25)(V_4Fe)_y (y=0, 0.02, 0.04, 0.06, 0.08) was investigated by substitution for partial Mn at 273 K, 293 K and 313 K. XRD results show that the alloys have C14 Laves phase structure and with increasing content, the lattice paramters of alloy are increased. PCT results show that substitution can increase the hydrogen storage capacity, decrease the plateau pressure and the hysteresis of the PCT. However, it can also increase the slope of the PCT. After being annealed at 1 223 K for 6 h, TiMn_(0.95)Cr_(0.25)(V_4Fe)_(0.06) alloy has a low desorption plateau pressure (1.04×10~5 Pa at 273 K and 2.72×10~5 Pa at 313 K) and a small hysteresis (0.14 at 273 K and 0.12 at 313 K). The maximum and effective hydrogen storage capacities are 2.0% and 1.75%(mass fraction) respectively, which are suitable for hydrogen storage tanks in PEMFC.
What problem does this paper attempt to address?