Effect of dew point temperature on surface selective oxidation behavior of Cu-bearing high strength steel

JIANG Guang-rui,WANG Hai-quan,TENG Hua-xiang,LIU Li-bin
DOI: https://doi.org/10.13289/j.issn.1009-6264.2017-0199
2017-01-01
Abstract:The annealing process of the high strength steel was simulated by a hot dip process simulator,and the samples were heated to the critical annealing temperature holding for 75 s then fast cooling to room temperature.The selective oxidation behavior at the external surface of the high strength steel during annealing was studied by means of scanning electron microscopy,glow discharge optical emission spectroscopyand X-ray photoelectron spectroscopy.The results show that the selective oxidation at the external surface of the steel is remarkably affected by the dew point temperature during annealing,and the higher dew point temperature (-10 ℃) can obviously inhibit the formation of oxides on the steel surface.The addition of 0.3 mass% copper to the tested steel can inhibit the formation of oxides of surface silicon and manganese and improve the inhibition effect.
What problem does this paper attempt to address?