Laser Cladding Stellite 6 + WC

钟敏霖,刘文今,陈艳霞,宁国庆
DOI: https://doi.org/10.3969/j.issn.1009-6264.2001.02.007
2001-01-01
Abstract:Laser cladding of Stellite+WC with WC volume rate of 0%, 9%, 18%, 27%, 36%, 45%, 54%, 72%, and 100% was investigated by dual powder feeding. The results demonstrated that no cracking happened until WC volume rate over 18%. The average hardness and cracking rate increased while height/width rate decreased with the increase of WC volume rate. The microstructure evolution can be divided into two domains. The first domain refers to WC volume rate from 0% to 36%, the WC added was completed melted and resolved into the melt pool and the re solidified structure dominated by the dendrite and interdendrite eutectic with W content respectively 9 68% and 21%. The second domain related to WC volume rate from 45% to 100%, in which most of the WC was melted and resolved, the microstructure dominated by the matrix and W compounds precipitated over it. The dissolution of W into the matrix was limited to maximum about 26%. The more the WC volume rate in the mixed powder, the more the precipitated W compound and the more W content within the W compound, which finally reached to 64 55%.
What problem does this paper attempt to address?