Synthesis of high vinyl solution polymerized styrene-butadiene rubber with three-peak distribution using mixed coupling agents

Wei XU,Ai-min LIANG,Yi-xian WU,Lin XU,Chuan-qing LI,Guo-zhu YU,Shi-chao WANG
DOI: https://doi.org/10.3969/j.issn.1000-1255.2014.04.004
2014-01-01
Abstract:High vinyl solution polymerized styrene-butadi-ene rubber( SSBR) was synthesized by batch copolymerization using cyclohexane/hexane as solvent , n-BuLi as initiator , ethyl tetrahydrofurfuryl ether ( ETE ) as modifier, (CH3)2SiCl2 and SiCl4 as mixed coupling agent.The modifi-er, mixed coupling agent and reaction condition were studied , and the properties comparison between the synthesized prod-uct and similar foreign product was conducted.The results showed that SSBR with high vinyl content and three-peak dis-tribution could be synthesized by using ETE as modifier , (CH3)2SiCl2 and SiCl4 as mixed coupling agent under the condition of the polymerization initiation temperature 35 ℃, mass fraction of monomer 13%, mass ratio of butadiene to styrene 74/26, ETE mass fraction (200 -250 ) ×10 -6 and the molar ratio of SiCl4 and (CH3)2SiCl2 0.34 to 0.36.The results of model and pilot tests showed that the properties of the synthesized product reached the level of similar foreign product.Silica was more suitable for being filler of silicon-modified SSBR.
What problem does this paper attempt to address?