Synthesis of SIBR in the Presence of BuLi/ TMEDA

WANG Qi-fei,WANG Ni-ni,SHI Gong-chang,LIAO Ming-yi,SHANG Yi-mei,YU Guo-zhu,LIANG Ai-min
DOI: https://doi.org/10.3969/j.issn.1005-3174.2005.05.003
2005-01-01
Abstract:The star-shaped styrene-butadiene-isoprene(SIBR)was synthesized with n-BuLi as initiator,coclohexane as solvent,TMEDA(N,N,N',N'-tetramethylethylene diamine)as polar modifier and SnCl_4 as coupling agent.The microstructure,molecular weight,molecular weight distribution,glass transition temperature and dynamic properties of synthesized SIBR were characterized by IR,GPC,DSC,DMA.The results showed that with the increase of TMEDA,the content of tans1,4-Bd and 1,4-Ip decreased clearly,the content of 3,4-Ip and the total content of 1,2 increased dramatically,and tanδ(0?℃)value increased obviously and all tanδ(60?℃)value were lower than 0.12.The mechanical properties of SIBR fit to the requests of tire tread,and dynamic properties of SIBR prospect potential application of high performance tires.