Location and Surface Species of Fluid Catalytic Cracking Catalyst Contaminants: Implications for Alleviating Catalyst Deactivation

U. J. Etim,Pingping Wu,Peng Bai,Wei Xing,Rooh Ullah,Fazle Subhan,Zifeng Yan
DOI: https://doi.org/10.1021/acs.energyfuels.6b02505
IF: 4.6541
2016-01-01
Energy & Fuels
Abstract:The deposition of appreciable amounts of metal poisons and carbon poses serious problems to the refiner during fluid catalytic cracking (FCC) unit operation. To check the effects of these contaminants on the catalyst, an in-depth understanding of their locations and existing states becomes necessary. In this work, the location and nature of vanadium, nickel, and coke species on the FCC catalyst were investigated. Detailed analyses of catalyst samples, including industrial equilibrium catalysts (E-cats), were accomplished using a variety of characterization techniques. It was found that nickel and vanadium concentrated mainly in meso- and micropores of the FCC catalyst, respectively. On the surface of E-cats, vanadium exists mainly in +4 and +5 oxidation states, while nickel is present as NiO, NiAl2O4, and surface nickel hydrosilicates and as NiO and NiAl2O4 in the bulk. The formation of a large amount of NiAl2O4 on the alumina support by nickel indicates its preferential location in the alumina component ...
What problem does this paper attempt to address?