Carbon Deposit Analysis in Catalyst Deactivation, Regeneration, and Rejuvenation.

B. Weckhuysen,E. Vogt,Donglong Fu
DOI: https://doi.org/10.1002/anie.202300319
2023-04-13
Angewandte Chemie
Abstract:Hydrocarbon conversion catalysts suffer from deactivation by deposition or formation of carbon deposits. Carbondeposit formation is thermodynamically favored above 350 °C, even in hydrogen-rich environments. We discuss four basic mechanisms: a carbenium-ion based mechanism taking place on acid sites of zeolites or bifunctional catalysts, a metal-induced formation of soft coke (i.e., oligomers of small olefins) on bifunctional catalysts, a radical-mediatedmechanism in higher-temperature processes, and fast-growing carbon filament formation. Catalysts deactivatebecause carbon deposits block pores at different length scales, or directly block active sites. Some deactivated catalysts can be re-used, others can be regenerated or have to be discarded. Catalyst and process design can mitigate the effects of deactivation. New analytical tools allow for the direct observation (in some cases even under in-situ or operando conditions) of the 3D-distribution of coke-type species as a function of catalyst lifetime.
Chemistry,Medicine,Materials Science
What problem does this paper attempt to address?