Eu2+, Mn2+, Sr2+ Tri-doped BaMgAl10O17 Phosphor: Solution Combustion Synthesis and Photoluminescence Properties

Zhang Chang-Wei,Ding Yan-Hua,Zhang Na,Zhang Jian-Yong,Fang Yong-Zheng,Zhang Cheng
DOI: https://doi.org/10.11862/CJIC.2016.237
2016-01-01
Chinese journal of inorganic chemistry
Abstract:Sr2+, Eu2+ and Mn2+ tri-doped BaMgAl10O17 (BAM) phosphors that emitting the blue-green light are prepared by solution combustion synthesis at 600 degrees C. X-ray diffraction (XRD), scanning electron microscopy (SEM) and photoluminescence (PL) are employed to measure the powders crystallinity, morphology and luminescent properties, respectively. The results show that the formation temperature of the BAM phase by the solution combustion synthesis (SCS) method is significantly lower than that of a high temperature solid state (HTS) reaction. The nanorods of SBAM: Eu2+, Mn2+ without aggregation and well distribution are synthesized successfully. The well-dispersed morphology of the SCS-derived phosphors is beneficial to the improvement of PL property. While Sr2+ ions are introduced, the PL property have been further enhanced, and the PL intensity can up to 1.8 times as high of that BAM specimen obtained by the HTS method. The xy CIE chromaticity coordinates of SBAM: 0.1Eu(2+), 0.04Mn(2+) phosphor is presented at (0.146, 0.250), located at the blue-green reign.
What problem does this paper attempt to address?