Study on Surface Morphology and Selectivity of Precipitated Iron Catalysts of FTS
Wang Xingjun,Gao Miao,Hong Bingqing,Shang Guofeng,Li Ping,Liu Yu,Wang Fuchen,Yu Zunhong
DOI: https://doi.org/10.1002/apj.325
2009-01-01
Asia-Pacific Journal of Chemical Engineering
Abstract:The precipitated iron catalyst was prepared by co-precipitation. The surface morphology of the catalyst was investigated under different reduction conditions by SEM (S-250, USA). Under H-2-reduction, the surface morphology of the catalyst had the obvious changes, which the diameter reduced, adhered together, came into being wads considered as a group. But the surface morphology of the catalyst had almost no change under CO reduction. The crystal structure of the catalyst was studied under different reduction conditions by X-ray diffraction (XRD) (Rigaku D/max, Japanese). It was found that the catalyst was reduced completely with H-2, but it was reduced partly with CO. The crystal structure of the catalyst converted into the metallic phase with H-2 reduction. However, most of the iron converted into iron oxide (Fe3O4) with CO reduction. And the predominant phase in a sample of a mature catalyst is chi-Fe5C2, which is the active phase in the Fischer-Tropsch synthesis (FTS). The experimental results showed that CO conversion and H-2 conversion increase with the change of reaction temperature from 260 to 300 degrees C, under the conditions of pressure P = 2.6 MPa, space velocity = 0.86 NI h(-1) g-Fe-1, n(H-2)/n(CO) = 2/3, and most of the hydrocarbon products are C5-11 which hold half of the hydrocarbon products. The next content is C2-4 which holds the quarter of hydrocarbon products. Then it is C12+, which is equal to 18%. And the last is C-1, which is equal to 7%. (c) 2009 Curtin University of Technology and John Wiley & Sons, Ltd.