SOLIDIFICATION CHARACTERISTICS OF RAPIDLY SOLIDIFIED HIGH SPEED STEEL POWDERS PRODUCED BY WATER ATOMIZATION

Wang Dongjun,Zhou Rui,Shen Jun
DOI: https://doi.org/10.3321/j.issn:0412-1961.2008.02.007
IF: 1.797
2008-01-01
ACTA METALLURGICA SINICA
Abstract:The cooling rate of the water atomized powders of M3/2 high speed steel was calculated to be 10~5—10~7 K/s.In the size range of the atomized powders,the microstructure consisted of equiaxed crystals and continuous network-like carbides between the equiaxed grains.The matrix of the powders was principally austenite;as the particle size decreased,the matrix changed from austenite to a composite consisting of austenite andδ-ferrite.The types of carbides were mainly cubic MC and close-packed hexagonal M_2C.
What problem does this paper attempt to address?