Corrosion Failure Analysis for Heat Transfer Tube in Quick Cooled Oil-Dilute Steam Heat Exchanger

CHEN Wen-jue,GU Fu-ming,SHI Sheng-fang,LU Bao-xi,YANG Zhen-guo
DOI: https://doi.org/10.3969/j.issn.1009-3281.2011.04.018
2011-01-01
Abstract:Several failure resulted from corrosion perforation occurred in tubes in heat exchanger have found in inspection in one petrochemical cooperation.The eddy current examination for tube bundle in heat exchanger was carried out.By using direct spectrum meter and 3-D microscope,the material of failed tube and concave surface were observed and examined.The composition of process water was also examined by using ion chromatogram meter and mass spectrum meter.Then,the broken edge and the hollow in tubes were analyzed from the observation of micro-surface and the analysis of the composition micro zone.It was shown that the cause of failure was resulted from calcium corrosion with local calcium congestion at concave zone and under scale.And the formation of alternate calcium and acid corrosion and the acid corrosion under scale may be other causes of the failure.
What problem does this paper attempt to address?