Sulfur-poisoning and Thermal Reduction Regeneration of Holmium-Modified Fe-Mn/TiO2 Catalyst for Low-Temperature SCR

Ke ZHUANG,Ya-ping ZHANG,Tian-jiao HUANG,Bin LU,Kai SHEN
DOI: https://doi.org/10.1016/s1872-5813(17)30060-9
2017-01-01
Journal of Fuel Chemistry and Technology
Abstract:The effect of SO2 on the low-temperature SCR activity and the thermal reduction regeneration for holmium-modified Fe-Mn/TiO2 catalyst were investigated by activity assessment and various characterization methods. The deposition of ammonium sulfate ( ( NH4 ) 2 SO4 ) on catalyst surface and the sulfuration of active component ( MnSO4 ) were proved to be the main causes for the deactivation in the presence of SO2 . The catalyst Fe0. 3 Ho0. 1 Mn0. 4/TiO2 exhibited superior SO2 durability when the concentration of SO2 was lower than 0. 04%, and the catalytic activity could markedly recover with the termination of sulfur-poisoning source. The deactivation behavior was irreversible when the concentration of SO2 was increased to 0. 1% but the poisoned catalyst could be regenerated after thermal reduction (350℃) for 60 min by 5% NH3 . The microstructure and physicochemical properties could be significantly restored after the thermal reduction regeneration. Moreover, the NOx conversion could return to about 80%.
What problem does this paper attempt to address?