Ultrafast Spectroscopic Identification Of Hole Transfer In All-Polymer Blend Films Of Poly(1-{4,8-Bis[5-(2-Ethylhexyl)Thiophen-2-Yl]-Benzo[1,2-B:4,5-B ']Dithiophen-2-Yl}-3-Methyl-5-(4-Octylphenyl)-4h-Thieno[3,4-C]Pyrrole-4, 6(5h)-Dione) And Poly[1,8-Bis(Dicarboximide)-2,6-Diyl]-Alt-5,5 '-(2,2 '-Bithiophene)]

Feng Jin,Jianyu Yuan,Wenping Guo,Lu Han,Yalong Xu,Chuanxiang Sheng,Wanli Ma,Haibin Zhao
DOI: https://doi.org/10.1021/acs.jpcc.7b04984
2017-01-01
Abstract:All-polymer solar cells composed of wide-band-gap polymer poly(1-{4,8-bis[5-(2-ethylhexyl)thiophen-2-yl]-benzo[1,2-b:4,5-b']dithiophen-2-yl}-3-methyl-5-(4-octylphenyl)-4H-thieno[3,4-c]pyrrole-4,6(5H)-dione) (PTP8) as the donor and poly[1,8-bis(dicarboximide)-2,6-diyl]-alt-5,5'-(2,2'-bithiophene)] [P(NDI2OD-T2), also known as Activink N2200] as the acceptor exhibit a broad absorbance in the range 300900 nm, thanks to complementary absorption of near-infrared light by N2200. Although N2200 shows reasonably high electron mobility, the contribution of the photogenerated excitons in N2200 to the power conversion of the PTP8/N2200 solar cell is insignificant. Here, the hole transfer from N2200 to PTP8 in PTP8/N2200 blend films was investigated by utilizing ultrafast transient absorption spectroscopy. The spectral fingerprints of ground-state bleaching and hole polaron-induced absorption of PTP8 are identified under selective excitation of the N2200 component and unambiguously indicate hole transfer from N2200 to PTP8. The hole transfer is slow (similar to 100 ps), comparable to the geminate exciton recombination rate, consequently limiting the transfer efficiency and carrier generation. The hole-transfer efficiency depends on the PTP8/N2200 weight ratio, showing a highest value of similar to 14.1% in the 3:2 film
What problem does this paper attempt to address?