Role of Cryogenic Temperature on the Strengthening Mechanism of Sicw-Al2o3 Composites

Weiwei Wu,Jingya Gui,Tianbin Zhu,Zhipeng Xie
DOI: https://doi.org/10.1016/j.ceramint.2016.06.152
IF: 5.532
2016-01-01
Ceramics International
Abstract:The flexural strength of SiCw-Al2O3 composites at cryogenic temperatures was investigated for the first time. The flexural strength of SiCw-Al2O3 composites measured at 77K was 874.66±72.64MPa, which was ∼29.5% higher than that at 293K. The strengthening mechanism of SiCw-Al2O3 composites at cryogenic temperatures could be attributed to the increase of elastic modulus, fracture surface energy and whisker/matrix interface strength. Also, the strengthening role of SiC whiskers was enhanced at cryogenic temperatures. So, SiCw-Al2O3 composites could be a promising material for applications in cryogenic environments.