Structural and thermal stabilities of spinel LiMn 2O 4 materials under commercial power batteries cycling and abusive conditions

Ling Guo-Wei,Zhu Xiping,He Yan-Bing,Song Quan-Sheng,Li Baohua,Li Yong-Jin,Yang Quan-Hong,Tang Zhi-Yuan
DOI: https://doi.org/10.1016/s1452-3981(23)13893-4
IF: 1.541
2012-01-01
International Journal of Electrochemical Science
Abstract:The commercial 18650 spinel LiMn 2O 4/graphite high power batteries are prepared and the structural and thermal stabilities of the spinel LiMn 2O 4 cathode materials under high rate cycling and abusive conditions are investigated using the commercial 18650 LiMn 2O 4/graphite high power batteries. Results show that the batteries present the best power performance when the compaction density of LiMn 2O 4 electrode is 2.93g cm -3. The microstructure of LiMn 2O 4 materials undergoes obvious distortion due to the Mn dissolution after the LiMn 2O 4 power batteries have been subjected to 100 cycles with discharge rate of 8 C at 25 °C and discharge rate of 5C at 55 °C. The charge-transfer resistance (R ct) of power batteries after cycling at high temperature rises significantly. During battery overcharge, the solid electrolyte interface (R sei) and R ct of power batteries increase greatly and the electrolyte shows obviously less reaction activities on LiMn 2O 4 electrode than on Li(Ni 1/3Co 1/3Mn 1/3)O 2 electrode. The reactions of fully charged LiMn 2O 4 cathodes and graphite anodes with electrolyte inside battery during battery overcharge and oven tests can be activated at much lower temperature than that outside battery, while these reactions do not occur during short current test in the fully charged batteries. © 2012 by ESG.
What problem does this paper attempt to address?