Low‐Temperature Preparation of Β‐si3n4 Porous Ceramics with a Small Amount of Li2O–Y2O3

Lei Fan,Meng Zhou,Hongjie Wang,Zhongqi Shi,Xuefeng Lu,Chao Wang
DOI: https://doi.org/10.1111/jace.12914
IF: 4.186
2014-01-01
Journal of the American Ceramic Society
Abstract:Porous β-Si3N4 ceramics are sintered at 1600°C in N2 and postheat treated at 1500°C under vacuum using Li2O and Y2O3 as the sintering additives. The partial sintering and phase transformation are promoted at low temperature by the addition of Li2O. The addition of Y2O3 is advantageous for the formation of high aspect ratio β-Si3N4 grains. After postheat treatment, a large amount of intergranular glassy phase is removed, and the Li content in the samples is decreased. By this method, the β-Si3N4 porous ceramic with a porosity of 54.1% and high flexural strength of 110 ± 8.1 MPa can be prepared with a small amount of sintering additives, 0.66 wt% Li2O and 0.33 wt% Y2O3, and it is suitable for high-temperature applications.