Dehydrogenation of Hydrogenated Ti-6Al-4V Alloy

Yuan Baoguo,Liu Dahai,Li Chunfeng
DOI: https://doi.org/10.1016/s1875-5372(14)60157-0
2014-01-01
Rare Metal Materials and Engineering
Abstract:TG/DSC tests of non-hydrogenated and hydrogenated Ti-6Al-4V alloys were carried out in order to investigate the dehydrogenation behavior of hydrogenated titanium alloys. Results indicate that mass losses of the hydrogenated Ti-6Al-4V alloys are significantly different with that of the non-hydrogenated Ti-6Al-4V alloy when the heating temperature is higher than 600 °C. Mass loss of the hydrogenated Ti-6Al-4V alloy increases with the increasing of hydrogen content when the heating temperature is in the range of 600 °C to 900 °C due to the decomposition of metastable phases. The maximum mass loss of the hydrogenated Ti-6Al-4V alloy is in correspondence with its hydrogen content upon no consideration of oxidation. The optimal dehydrogenation temperature among hydrogenated Ti-6Al-4V alloys is 750 °C. The dehydrogenation process for all hydrogenated Ti-6Al-4V alloys is the same.
What problem does this paper attempt to address?