Thermal deformation behavior of γ-TiAl based alloy by plasma hydrogenation

Fuyu Dong,Yongda Liu,Yue Zhang,Weidong Li,Peter K. Liaw,Minghao Shi,Hongjun Huang,Xiaojiao Zuo,Liangshun Luo,Yanqing Su,Jun Cheng
DOI: https://doi.org/10.1016/j.ijhydene.2020.09.008
IF: 7.2
2020-11-01
International Journal of Hydrogen Energy
Abstract:<p>The Ti–48Al–2Cr alloy was subjected to the plasma-hydrogenation treatment. Then the alloy containing minor hydrogen was prepared (0.058 wt percent, wt.%). Hot-compression experiments were carried out at temperatures ranging from 1000 to 1,150 °C and strain rates ranging from 1 to 0.001 s<sup>−1</sup>. The results show that the peak stress after the plasma-hydrogenation treatment is lower than that of the unhydrogenated one. At 1100 °C and the strain rate of 0.01 s<sup>−1</sup>, the peak stress is reduced by 32.3%. The mechanism of high-temperature softening caused by plasma-hydrogenation is examined, and the constitutive equations are established for the unhydrogenated and hydrogenated alloys. Through the constitutive equations, the high-temperature softening mechanism of unhydrogenated and hydrogenated alloys are dynamic-recrystallization, and the activation energy of hydrogenated alloy is lower than that of the unhydrogenated. Meanwhile, electron back-scatter diffraction analyses of the thermal-compressed microstructures show that the hydrogenated alloy has more recrystallized grains, less lamellar structure, and more uniform deformation than the unhydrogenated alloy.</p>
energy & fuels,electrochemistry,chemistry, physical
What problem does this paper attempt to address?