Sintering Temperature and Impedance Analysis of Mn0.9co1.2ni0.27mg0.15al0.03fe0.45o4 Ntc Ceramic Prepared by W/O Microemulsion Method

Junbo Xia,Qing Zhao,Bo Gao,Aimin Chang,Bo Zhang,Pengjun Zhao,Renjun Ma
DOI: https://doi.org/10.1016/j.jallcom.2014.07.149
IF: 6.2
2014-01-01
Journal of Alloys and Compounds
Abstract:The Mn0.9Co1.2Ni0.27Mg0.5Al0.03Fe0.45O4 negative temperature coefficient (NTC) ceramics derived from nano-particles were sintered at 1380 degrees C, 1450 degrees C and 1560 degrees C, respectively. X-ray diffraction (XRD) result showed that the ceramics sintered at 1380 degrees C and 1450 degrees C were mainly in the cubic spinel structure except for a little of tetragonal spinel, and that sintered at 1560 C was consisted of cubic spinel and cubic cobalt oxide phase. Scanning electron microscopy (SEM) image indicated that the grain size of the ceramic increased sharply when the sintering temperature increased from 1380 degrees C to 1450 degrees C, and it changed little when the temperature further increased to 1560 degrees C, while the porosity was enlarged seriously. Thus a perfect sintering temperature of 1450 degrees C was proposed. Impedance analysis revealed that the grain resistance R-g showed positive temperature coefficient thermistor characteristic, while the grain boundary resistance R-gb possessed negative temperature coefficient characteristic. Because the grain boundary resistance R-gb was two orders of magnitude larger than the grain resistance R-g, the material thus showed negative temperature coefficient thermistor characteristic. (C) 2014 Elsevier B.V. All rights reserved.
What problem does this paper attempt to address?