Structure and Electrical Performance of Mn1.5−0.5xCo0.9−0.3xNi0.6−0.2xCuxO4 NTC Ceramics Prepared by Heterogeneous Precipitation

Kai Xiong,Shi-Xi Zhao,Deng-Feng Li,Han-Qing Bao,Ce-Wen Nan
DOI: https://doi.org/10.1016/j.jallcom.2014.04.019
IF: 6.2
2014-01-01
Journal of Alloys and Compounds
Abstract:The spinel-structured ceramics of Mn1.5-0.5xCo0.9-0.3xNi0.6-0.2xCuxO4 negative temperature coefficient (NTC) thermistors were fabricated by heterogeneous precipitation. The precursor powder of Mn1.5Co0.9 Ni0.6O4 was first prepared by mixing manganese, cobalt and nickel oxide with a molar ratio of 5:3:2 and calcining at 1100 degrees C for 2 h. Cupric carbonate was precipitated onto the surface of the precursor particles by heterogeneous precipitation, and then the powder was pressed and sintered. The Cu-precipitated powders were confirmed by both TGA/DSC analysis and SEM images. The microstructures of the ceramics were predominantly spinel structure and a small amount of NiO rock-salt. In comparison with the samples of the same composition prepared by traditional solid-state methods, ceramics from heterogeneous precipitation powder demonstrate lower electrical resistivity, higher B constants and much better electrical stability. (c) 2014 Elsevier B.V. All rights reserved.
What problem does this paper attempt to address?